http://data.posccaesar.org/rdl/RDS611324
| hasCreationDate | 1999.04.23 |
|---|---|
| hasCreator | u20418 |
| hasDefinition | Austenitic Cr-Ni Heat Resisting Steel (309HCb) assigned with S30941 of the Unified Numbering System (UNS) for metals and alloys in accordance to the standard practice ASTM E 527-83 (Reapproved 1991). |
| hasDesignation | UNS S30941 |
| hasDesignationAbbrev | 4864100 |
| hasIdPCA | RDS611324 |
| hasNote | Cb is an equivalent for Nb. Chemical composition limits for UNS S30941 are as follows in wt%: C 0.04-010 Cr 22.00-24.00 Cu 0.75 max Mn 2.00 max Mo 0.75 max Nb+Ta 10xC-1.10 Ni 12.0-16.0 P 0.040 max S 0.030 max Si 0 |
| hasStatus | Candidate |
| Resource | Via |
|---|---|
| RDS13000158 | hasSubclass |
| RDS3859060 | hasSubclass |
| RDS3859077 | hasSubclass |
| RDS3859196 | hasSuperclass |
| RDS3885733 | hasSuperclass |
| RDS5907864 | hasClassified |
| RDS999827008 | hasRepresented |