http://data.posccaesar.org/rdl/RDS611999
| hasCreationDate | 1999.04.23 |
|---|---|
| hasCreator | u20418 |
| hasDefinition | Austenitic Cr-Ni Heat Resisting Steel (310HCb) assigned with S31041 of the Unified Numbering System (UNS) for metals and alloys in accordance to the standard practice ASTM E 527-83 (Reapproved 1991) |
| hasDesignation | UNS S31041 |
| hasDesignationAbbrev | 4941400 |
| hasIdPCA | RDS611999 |
| hasNote | Cb is equivelent with Nb. Chemical composition limits for UNS S31041 are as follows in wt%: C 0.08-0.10 Cr 24.0-26.0 Cu 0.75 max Mn 2.00 max Mo 0.75 max Nb+Ta 10xC-1.10 Ni 19.0-22.0 P 0.045 max S |
| hasStatus | Candidate |
| Resource | Via |
|---|---|
| RDS13000243 | hasSubclass |
| RDS3863803 | hasSubclass |
| RDS3863820 | hasSubclass |
| RDS3865469 | hasSuperclass |
| RDS3885801 | hasSuperclass |
| RDS5907779 | hasClassified |
| RDS999828852 | hasRepresented |