http://data.posccaesar.org/rdl/RDS616004
| hasCreationDate | 1996.11.27 |
|---|---|
| hasCreator | u82302 |
| hasDefinition | Structural steel assigned with the material name S275M in accordance with the designation system of the European Standard EN 10027-1:1992, with a minimum yield strength of 275 MPa for the smallest thickness range and thermomechanical rolled. |
| hasDesignation | S275M |
| hasDesignationAbbrev | 5084700 |
| hasIdPCA | RDS616004 |
| hasNote | The steel has the number 1.8818 in accordance with EN 10027-2:1992. |
| hasStatus | Recorded |
| Resource | Via |
|---|---|
| RDS12996422 | hasSubclass |
| RDS3870144 | hasSubclass |
| RDS3870739 | hasSuperclass |
| RDS5939562 | hasClassified |
| RDS999807503 | hasRepresented |