http://data.posccaesar.org/rdl/RDS616229
| hasCreationDate | 1996.11.25 |
|---|---|
| hasCreator | u82302 |
| hasDefinition | Steel assigned with the material name S420ML in accordance with the designation system of the European Standard EN 10027-1:1992, with a minimum yield strength of 420 MPa for the smallest thickness range, thermomechanical rolled and applicable for low temperature service. |
| hasDesignation | S420ML |
| hasDesignationAbbrev | 5086600 |
| hasIdPCA | RDS616229 |
| hasNote | The steel has the number 1.8836 in accordance with EN 10027-2:1992. |
| hasStatus | Recorded |
| Resource | Via |
|---|---|
| RDS12996507 | hasSubclass |
| RDS3870501 | hasSubclass |
| RDS3870824 | hasSuperclass |
| RDS5938712 | hasClassified |
| RDS999807825 | hasRepresented |