← Search

S275J0

ClassOfCompound

http://data.posccaesar.org/rdl/RDS617264

hasCreationDate1996.11.25
hasCreatoru82302
hasDefinitionStructural steel assigned with the material name S275J0 in accordance with the designation system of the European Standard EN 10027-1:1992, with a minimum yield strength for the smallest thickness range of 275 MPa and impact property of minimum 27 J at 0 degr. Celsius.
hasDesignationS275J0
hasDesignationAbbrev5112500
hasIdPCARDS617264
hasNoteThe steel has the number 1.0143 in accordance with EN 10027-2:1992.
hasStatusRecorded

Referenced by (4)

ResourceVia
RDS3871215hasSubclass
RDS3871776hasSuperclass
RDS5939409hasClassified
RDS999808046hasRepresented