| hasNote | Based on: 1) The steel making process shall be the Basic Oxygen or Basic Electric Arc Furnace process, fully killed and fine grained. 2) Product analysis. 3) Modified chemical composition of S335NLO2. 4) Limited to Normalised. 5) Impact testing in transverse direction at -40 degree Celcius. 6) The thickness limitation is for plates up to and including 150 mm, sections up to and including 63 mm, seamless hollow sections up to and including 40 mm, and resistance welded hollow sections up to and including 20 mm. |