| hasNote | Based on: 1) The steel making process shall be by a low sulphur and phosphorus refining process in a Basic Oxygen or Basic Electric Arc Furnace, fully killed, fine grained, vacuum degassed or ladle refined. 2) Product analysis 3) Limited to Normalised. 4) Impact testing in transverse direction at -40 degree Celcius. 5) The thickness limitation is for plates up to and including 150 mm, sections up to and including 63 mm, seamless hollow sections up to and including 40 mm, and resistance welded hollow sections up to and including 20 mm. |