http://data.posccaesar.org/rdl/RDS630089
| hasCreationDate | 1999.04.23 |
|---|---|
| hasCreator | u20418 |
| hasDefinition | Austenitic Cr-Ni Stainless Steel, High Nitrogen, assigned with S30452 of the Unified Numbering System (UNS) for metals and alloys in accordance to the standard practice ASTM E 527-83 (Reapproved 1991) |
| hasDesignation | UNS S30452 |
| hasDesignationAbbrev | 5519400 |
| hasIdPCA | RDS630089 |
| hasNote | Chemical composition limits for UNS S30452 are as follows in wt%: C 0.08 max Cr 18.00-20.00 Mn 2.00 max N 0.16-0.30 Ni 8.00-10.50 P 0.045 max S 0.030 max Si 1.00 max |
| hasStatus | Candidate |
| Resource | Via |
|---|---|
| RDS3882588 | hasSubclass |
| RDS3882605 | hasSubclass |
| RDS3882622 | hasSubclass |
| RDS3885291 | hasSuperclass |
| RDS5908051 | hasClassified |
| RDS999826758 | hasRepresented |