← Search

UNS S30500

ClassOfCompound

http://data.posccaesar.org/rdl/RDS630134

hasCreationDate1999.04.23
hasCreatoru20418
hasDefinitionAustenitic Cr-Ni Stainless Steel (Low work hardening) assigned with S30500 of the Unified Numbering System (UNS) for metals and alloys in accordance to the standard practice ASTM E 527-83 (Reapproved 1991).
hasDesignationUNS S30500
hasDesignationAbbrev5519500
hasIdPCARDS630134
hasNoteChemical composition limits for UNS S30500 are as follows in wt%: C 0.12 max Cr 17.00-19.00 Mn 2.00 max Ni 10.00-13.00 P 0.045 max S 0.030 max Si 1.00 max
hasStatusCandidate